Sign In | Join Free | My portofva.com |
|
Brand Name : ZW
Model Number : cast ball,forged ball
Certification : ISO9001:2008 SGS
Place of Origin : CHINA
MOQ : 1
Price : Negotiable
Payment Terms : L/C, D/A, D/P, T/T, Western Union, MoneyGram
Supply Ability : 50000 tons/year
Delivery Time : 7-14 days
Packaging Details : container bags or steel drums
Breakage Guarantee : ≤1%
HRC : cast ball 45-50,forged ball 50-65
Name : grinding ball for ballmill
Impact Test : ≥4 AK.j/cm^2
Quality system authentication : ISO9001:2008/SGS TEST REPORT
Endurance Test Times : ≥10000
Forged ball and cast ball grinding balls for ball mill size 20mm-150mm
Specifications of our products as follows:
Type and Chenical Composition of Cast Balls
| | Chemical Composition | ||||||
C | Si | Mn | S/P | Cr | HRC | |||
Cast ball | special hi-cr | 2.0-3.2 | <1.0 | 0.5-2.0 | <0.06 | >18 | 58-64 | |
higt-cr | 2.0-3.2 | <1.0 | 0.5-1.5 | <0.06 | >10 | 58-62 | ||
| 2.0-3.2 | <1.0 | 0.5-1.5 | <0.06 | ≥5 | 45-48 | ||
| 2.2-3.4 | ≤1.2 | 0.5-1.5 | ≤0.06 | 1.0-1.5 | 42-46 |
Physical property of cast iron balls
Name
| Material | Impact test AK.j/cm^2 | Endurance test times | HRC | Breakage |
Cast ball
| special hi-cr | ≥4 | ≥10000 | 58-64 | <1% |
higt-cr | ≥3 | ≥10000 | 58-62 | <1% | |
medium-cr | ≥3 | ≥8000 | 45-48 | <1% | |
low-cr | ≥2 | ≥8000 | 42-46 | <1% |
.Electric furnace smelting:All cast steel balls are produced by intermediate frequency electric furance .The purity and stability of materials are effectively esured after unform temerature conditioning and twice hot metal purificati0n.
.Assay before furnace :Temperature control is an important and complex process during cast steel ball production.Different tapping temperature and heat temperature are sensitively reflected in the quality of the products.It is requested to master the proper pouring temperature ,mold temperature ,so that can make sure the products achieve a good state of body tisssue during the transition from Liquid to solid states.
Process features of cast iron balls:
Moulding process---pouing when the molten iron temoerature reaches 1500 C,using the teoperature difference between moletn iron and the molds.in this way,the ball can achieve internal organization of grain refinement and be moredense.menanwhile,the carvide is radially arranged .and such carbide is embedded in the matrix again during grinding process,forming hatd layer continously,so that the hardness and toughness is maintained to a reasonable range,greatly improving the toughness and hardness of the grinding balls.
![]() |